causes
|
Influence on processing shrinkage
|
|
lessening
|
increasing
|
|
Density increase due to thermal contraction by cooling the demoulding temperature to room temperature and compression by the action of pressure
|
- high effective pressure on moulding compound and contour until demoulding (holding pressure)
- low demoulding temperature (long cooling time and/or low contour temperature)
- low coefficient of thermal expansion (hard elastic polymers)
|
- low or prematurely reduced holding pressure until demoulding
- high demoulding temperature (short cooling time and/or high contour temperature)
- high coefficient of thermal expansion (soft or rubber-elastic polymers)
|
|
Density increase due to thermodynamically induced structural order processes (crystallization; gelation)
|
- amorphous polymers
- ow degree of crystallinity of semi-crystalline polymers due to rapid solidification (subcooling due to low contour temperature and/or thin-walled parts)
- high degree of gelation of polymers containing plasticizers
|
- semi-crystalline polymers
- high degree of crystallinity due to slow solidification (high contour temperature and/or thick-walled parts) and improved nucleation (nucleation additives)
- low degree of gelation of polymers containing plasticizers
|
|
Density increase due to molecular construction and cross-linking processes (curing; vulcanization; polyreaction)
|
- high degree of cross-linking and thus lower coefficient of thermal expansion (long curing or vulcanization time and/or high melt temperature)
- Preformed or pre-crosslinked molding compounds (e.g. prepolymers)
|
- low degree of cross-linking and thus higher coefficient of thermal expansion (short curing or vulcanization time and/or low melt temperature)
- non-crosslinked precursors (oligomers) or monomers as moulding compositions
|
|
Changes in stiffness or hardness due to additives (e.g. fillers and reinforcing materials; plasticizers)
|
- Additives with low coefficient of thermal expansion (e.g. inorganic fillers and reinforcing materials)
- no or low plasticizer additives
|
- Additives with high coefficient of thermal expansion (e.g. organic fillers and reinforcing materials)
- plasticizer additives
|